Quick Answer
Material selection for casting alloys — choose based on application requirements: strength, corrosion resistance, wear resistance, machinability, cost, and casting process fit. Gray iron for damping and low cost; ductile iron for strength and toughness; aluminum for lightweight and corrosion; carbon steel for strength at low cost; stainless steel for corrosion and high temperature; bronze/brass for bearing surfaces and corrosion.
Key Selection Factors
| Factor | What to Consider | How to Evaluate |
|---|---|---|
| Mechanical strength | Yield strength, tensile strength, fatigue strength, impact resistance | Mechanical test data from material cert |
| Corrosion resistance | Environment: fresh water, salt water, chemicals, atmosphere, temperature | Alloy selection for environment; test data |
| Wear resistance | Abrasive wear, adhesive wear, impact wear | Hardness, microstructure |
| Machinability | How easy to machine after casting | Machinability rating, tool wear, chip formation |
| Cost | Material + processing + tooling + machining | Total cost per part vs. performance |
| Casting process fit | Can this alloy be cast by the required process? | Castability, fluidity, solidification range |
| Weight | Density; critical for automotive, aerospace, portable | Compare density (Al 2.7, Fe 7.2, Cu 8.9 g/cm³) |
| Thermal properties | Thermal conductivity, high temperature resistance | Heat sink, furnace, exhaust applications |
Gray Iron (Gray Cast Iron)
Properties: Excellent damping (vibration absorption), good wear resistance, excellent thermal stability, low cost.
Limitations: Brittle, low tensile strength, poor weldability, cannot be heat treated for strength.
| Grade | Tensile Strength | Best For |
|---|---|---|
| Class 20 | 140 MPa | General purpose, low stress |
| Class 30 | 210 MPa | Machine bases, housing |
| Class 40 | 280 MPa | Engine blocks, brake rotors |
Applications: Engine blocks, machine bases, brake rotors, gear housings, pump bodies.
Ductile Iron (Nodular Cast Iron)
Properties: High strength + ductility, excellent impact resistance, good fatigue strength, weldable.
Limitations: More expensive than gray iron, requires controlled casting process.
| Grade | Yield Strength | Elongation | Best For |
|---|---|---|---|
| 60-40-18 | 400 MPa | 18% | High ductility applications |
| 65-45-12 | 450 MPa | 12% | General purpose |
| 80-60-03 | 600 MPa | 3% | High strength applications |
Applications: Automotive suspension components, gears, crankshafts, structural parts, pressure fittings.
Aluminum Casting Alloys
Properties: Lightweight (2.7 g/cm³), excellent corrosion resistance, good thermal conductivity, castable by multiple processes.
Limitations: Lower strength than steel/iron, limited high temperature capability.
| Alloy | Process | Key Properties | Applications |
|---|---|---|---|
| A356 | Sand, investment, gravity die | Good strength, excellent castability | Automotive, aerospace, general |
| A380 | High pressure die casting | Excellent castability, moderate strength | Complex thin-wall parts, housings |
| 6061 (wrought equivalent) | Sand casting | Good strength, weldable | Structural parts |
Applications: Automotive parts, aerospace components, heat sinks, electronic housings, marine hardware.
Carbon Steel Castings
Properties: High strength, low cost, weldable, heat treatable for higher strength.
Limitations: Needs coating for corrosion, higher density than aluminum.
| Grade | Yield Strength | Best For |
|---|---|---|
| WCB | 240 MPa | General purpose, pressure fittings |
| WCC | 280 MPa | Higher strength applications |
| LCC | 350 MPa | Low temperature service |
Applications: Structural parts, machinery components, pressure fittings, railway components.
Stainless Steel Castings
Properties: Excellent corrosion resistance, good high temperature capability, good strength.
Limitations: Higher cost, harder to machine, some grades difficult to cast.
| Cast Grade | Wrought Equivalent | Best For |
|---|---|---|
| CF8 | 304 | General corrosion resistance, food processing |
| CG8M | 316 | Marine, chemical, medical applications |
| CK20 | 310S | High temperature furnace parts |
Applications: Marine hardware, chemical processing, medical devices, food processing, high temperature parts.
Bronze and Brass Castings
Properties: Excellent corrosion resistance (marine), good bearing properties, excellent machinability.
Limitations: Higher cost, lower strength than steel/iron, high density.
| Alloy | Key Properties | Applications |
|---|---|---|
| C93200 (bearing bronze) | Excellent bearing properties | Bearing sleeves, bushings |
| C95400 (aluminum bronze) | High strength, corrosion resistant | Marine hardware, pump parts |
| C83600 (red brass) | Good corrosion, excellent machinability | Valves, fittings, decorative |
Applications: Bearings, bushings, marine hardware, valve components, pump parts, decorative hardware.
Buyer Decision Checklist
- What is the primary application requirement (strength, corrosion, wear, weight)?
- What is the service environment (temperature, chemicals, atmosphere)?
- What casting process is required (sand, investment, die)?
- What is the realistic budget per part?
- Is machining required after casting? How does machinability affect cost?
- Is welding required? Which alloys are weldable?
- What is the expected service life?
- Has the foundry confirmed this alloy is castable by the required process?
Before finalizing the sourcing decision, many OEM buyers also compare Sand Casting, Aluminum Casting Buyer Guide, and Cast Iron vs Cast Steel to clarify process fit, cost trade-offs, tolerance expectations, and supplier risk.
If you need application-specific guidance, drawing review, or a quotation, you can Contact YCUMETAL.
Engineering & Sourcing Tools: Use our ASTM vs EN/DIN vs JIS vs GB Casting Grade Cross-Reference Calculator and ISO 8062 CT4–CT12 Casting Tolerance & RMA Chart to verify specifications, or explore YCUMETAL’s precision investment casting, 3/4/5-axis CNC machining, industrial automation & robotics components, and full foundry services (request a 24h DFM quote).
FAQ
Which casting alloy is cheapest?
Gray iron for ferrous applications; aluminum A380 for lightweight applications. Gray iron is typically the lowest-cost casting alloy.
Which alloy for corrosion resistance?
Stainless steel (CF8/CG8M) for general corrosion; aluminum for atmospheric corrosion; bronze/brass for marine corrosion.
Which alloy for high strength?
High-grade ductile iron (80-60-03) or carbon steel castings (LCC) for cost-effective strength. For highest strength with corrosion, stainless steel castings.
Related Casting & CNC Engineering Guides (Aluminum Gravity, Die & Sand Casting Grades (ADC12 / A380 / A356-T6))
Core Process & Industry Hubs: Aluminum Gravity & Die Casting Service • Automotive Aluminum Castings • ADC12 vs A380 vs A356 Aluminum Casting Alloys: Composition, T6 Strength & Process Selection • ASTM / EN / JIS / GB Grade Cross-Reference Tool • ISO 8062 CT4–CT12 Tolerance Chart
- Surface Treatment for Aluminum Castings: How OEM Buyers Choose Anodizing, Powder Coat, Paint, Plating, and Polishing
- Aluminum Alloy Selection for Castings: How OEM Buyers Choose the Right Aluminum Casting Alloy
- Die Casting Tooling Cost: How OEM Buyers Budget for Dies, Patterns, and Molds
- Die Casting Design: How OEM Buyers Design Parts That Die Casting Can Produce Successfully
- Aluminum Casting: A Complete Buyer Guide to Processes, Alloys, and Sourcing for OEM Parts
- Permanent Mold Casting: How OEM Buyers Source Metal Parts Made with Reusable Steel Dies
Frequently Asked Engineering Questions
Which casting alloy is cheapest?
Which alloy for corrosion resistance?
Which alloy for high strength?
Aluminum & Non-Ferrous Foundry Engineering Specifications: Melt Treatment, Porosity Control & T6 Aging
In high-reliability B2B production of light-alloy components related to Cast Aluminum vs Cast Iron: How OEM Buyers Choose Between Aluminum and Iron Castings, foundry metallurgical control begins before pouring. Molten aluminum alloys (such as A356.0 / AlSi7Mg0.3, A380.0 / ADC12, and 319.0) readily absorb dissolved atomic hydrogen from atmospheric moisture above 680°C. At Qingdao Yucheng’s 34,000 m² facility, every furnace charge undergoes rotary argon/nitrogen degassing and ceramic foam filtration (20–30 PPI) until reduced-pressure test (RPT) density index values drop below 1.5%. For structural castings requiring T6 solution heat treatment (535–540°C solutionizing for 6–8 hours, polymer/warm-water quench at 60–80°C, and artificial aging at 155–170°C), permanent mold gravity casting or low-pressure die casting is prioritized over conventional high-pressure die casting (HPDC) to prevent subsurface gas blistering.
| Material / Process Specification | Applicable Standard & Production Route | Mechanical / Dimensional Capability | Quality Verification & Deliverable |
|---|---|---|---|
| A356-T6 (EN AC-42100 / AC4CH / ZL101A) | Gravity Die / Low-Pressure / Resin Sand | UTS ≥290 MPa | Yield ≥210 MPa | El ≥5% | 85–95 HB | ISO 8062 CT6–CT7; X-ray ASTM E155 Level 2 |
| A380 / ADC12 (EN AC-46000 / AlSi9Cu3) | High-Pressure Die Casting (HPDC) + CNC | UTS ≥310 MPa | Yield ≥160 MPa | El 2–3% | 80 HB | ISO 8062 CT5–CT6; thin walls down to 1.8 mm |
| AZ91D Magnesium / ZA-8 & Zamak 3 Zinc | SF6/N2 Protected Low-Pressure / Chamber HPDC | UTS 230–295 MPa | Yield 150–220 MPa | Low density | CT5–CT6; chromate-free passivation + powder coat |
B2B Cost Drivers, Tooling Amortization, Low-MOQ Prototyping & RFQ Checklist
When comparing quotes across custom metal casting and CNC machining manufacturers, unit piece price alone rarely reflects total landed cost. Engineering and purchasing teams evaluating Cast Aluminum vs Cast Iron: How OEM Buyers Choose Between Aluminum and Iron Castings optimize total cost of ownership (TCO) across four operational levers:
- 1. Rapid Prototyping vs. Hard Tooling Break-Even Analysis: For pilot validation runs of 5 to 50 pieces, 3D-printed PMMA/SLA wax patterns (for investment casting) or CNC-machined resin-sand / hog-out billets eliminate $1,500–$4,500 in initial permanent tooling investment and compress T1 sample delivery to 10–14 calendar days. Once annual volume exceeds 150–300 pieces, dedicated aluminum wax dies, metal shell patterns, or H13 steel permanent molds amortize within the first production batch while cutting unit casting cost by 35–55%.
- 2. Near-Net-Shape Coring to Eliminate Secondary CNC Cycle Time: Every millimeter of excess machining stock adds spindle minutes, insert wear, and chip waste. By designing soluble/ceramic cores or precision shell cores into internal fluid passages, clevis slots, and weight-saver pockets, required machining allowance (RMA) is restricted strictly to functional sealing faces, H7 bearing bores, and threaded ports.
- 3. Heat-Lot Traceability & Defect Containment (Zero-Defect Gateways): Each production batch is tracked via a unique heat/pour barcode from raw charge make-up through spectrometer chemistry verification, T6/normalizing heat-treatment furnace charts, shot-blasting, CNC probing, and pressure leak testing. Full EN 10204 3.1 mill certificates and ballooned CMM dimensional reports accompany every shipment.
- 4. Export Packaging & Sea/Air Freight Corrosion Prevention: Machined ferrous and aluminum surfaces are protected with vapour-phase corrosion inhibitor (VCI) film, desiccant packs, and custom-slotted ISPM-15 fumigation-free plywood crates engineered to withstand 45-day ocean transit without fretting or surface oxidation.
What to Include in Your Technical RFQ Package: To receive a comprehensive DFM review and itemized tooling + piece-price breakdown within 24 hours from Qingdao Yucheng’s engineering team, please provide: (1) 3D CAD model (STEP / IGES / Parasolid) + 2D PDF drawing with GD&T tolerances; (2) target material grade (ASTM / EN / DIN / JIS / GB); (3) estimated batch quantity and annual usage (EAU); (4) required surface finish or coating specification; and (5) any special NDT (X-ray, UT, MT, PT, pressure test) or PPAP documentation requirements.